AASHTO R 93 – Standard Practice for Service Life Determination of Corrugated HDPE Pipes Manufactured with Recycled Content

AASHTO R 93-19 details the procedure for determining the service life of corrugated highdensity polyethylene (HDPE) pipes containing recycled materials. Service life is relative to Stage II brittle failures via the slow crack growth mechanism.

The service life determination in this standard practice is based on analysis of failure data from testing conducted in accordance with ASTM F3181, the Un-Notched Constant Ligament Stress (UCLS) test.

This standard practice can be used to establish minimum UCLS performance criteria to ensure a desired service life at given service conditions for corrugated HDPE pipes containing recycled materials.

This standard practice is applicable for pipes containing recycled materials and manufactured in accordance to AASHTO M 294. It is applicable both for pipes manufactured with post-consumer recycled (PCR) materials and post-industrial recycled (PIR) materials. It is not intended for pipes manufactured with only virgin materials.

Product Details

Published:
2019
Number of Pages:
10
File Size:
1 file , 2 MB
Product Code(s):
R093-19-UL, R093-19-UL, R093-19-UL
Note:
This product is unavailable in Ukraine, Russia, Belarus